Low Alloy High Strength Q370R Steel Plate

Low Alloy High Strength Q370R Steel Plate

Thickness:3-150mm
Width:1220-4200mm
Length:5000-18000mm
Sende bookingforespørsel
Chat nå
Beskrivelse
Tekniske parametere

Low Alloy High Strength Q370R Steel Plate

 

product-570-424

GBT713 Q370R vessel steel plates are suitable for pressure vessel compression components at middle and normal temperatures. The thickness of Q370R vessel steel plates is 6mm~180mm. GBT713 Q370R vessel steel plates are used for the manufacture of petroleum, chemical, gas separation, gas storage and transportation containers or other similar preparations, such as various towers, heat exchangers, tanks, tankers and so on.

 

Q370R Chemical composition

 

C %

V %

Q370R

0.18

0.55

1.2-.1.7

0.3

0.3

0.3

0.08

0.05

P %

S %

 

 

 

0.03

0.02

0.025

0.010

0.015-0.05

 

 

 

 

Q370R Mechanical Property

 

 

 

 

 

 

Q370R

10-16

370Mpa

530-630 Mpa

20%

-20

47J

16-36

360 Mpa

530-630 Mpa

20%

-20

47J

36-60

340 Mpa

520-620 Mpa

20%

-20

47J

60-100

330 Mpa

510-610 Mpa

20%

-20

47J

 

 

: The combination of top-bottom combined blowing converter smelting, LF refining, and RH vacuum circulation degassing is adopted to control the purity of molten steel. The total amount of non-metallic inclusions is <= grade 2.0, which is 40% lower than that of traditional processes.

 

: Through the controlled rolling and controlled cooling (TMCP) technology, a fine-grained ferrite + pearlite structure is obtained at the final rolling temperature of 850-950℃. Combined with normalizing treatment at 680℃, the tensile strength of the steel plate reaches 530-630MPa, and the elongation is >=20%.

 

: The GB/T 713-2023 standard is implemented. Ultrasonic flaw detection meets grade III qualification by default, and the thickness deviation conforms to the provisions of Class B, ensuring 100% traceability of products.

 

 

 

The steel sheet will be packed in seaworthy packing such as steel strips bundles. If you have any special requests on this, please let us know advanced. We will refer to your email kindly.
product-440-218
1).20ft GP:5898mm(Length)x2352mm(Width)x2393mm(High)

2).40ft GP:12032mm(Length)x2352mm(Width)x2393mm(High)

3).40ft HC:12032mm(Lengh)x2352mm(Width)x2698mm(High)

 

 

 

 and any requirement in steel material, please feel free to contact us.

 

GB/T 713 Q370R NACE MR0175, MR0103 Boiler steel plate, Low alloy and high strength steel plate, heavy plate and wide, heavy plate.

 

alloy@gneesteelgroup.com. We are more than happy to assist you.

Populære tags: low alloy high strength q370r steel plate, China low alloy high strength q370r steel plate manufacturers, suppliers, factory