1Cr5Mo steel is a martensitic metal structure.1Cr5Mo has good oxidation resistance around 650 degree , good thermal strength below 600 degree , and good vibration damping and thermal conductivity.1Cr5Mo steel is widely used in steam turbines.15CrMo steel plate is a heat-resistant steel with pearlitic structure.15CrMo steel plate is a heat-resistant steel with pearlitic structure.
15CrMo steel plate is a kind of heat-resistant steel with pearlitic structure, with high thermal strength (δb Greater than or equal to 440MPa) and high-temperature oxidation resistance, and a certain degree of hydrogen corrosion resistance. Due to the high content of Cr, C and other alloying elements in the steel, the steel hardening tendency is obvious, and the weldability is poor.
Chemical composition and chemical elements of 1Cr5Mo and 15CrMo steel plate:
| C | P | S | |||||||
| 1Cr5Mo | Less than or equal to 0.15 | Less than or equal to 0.50 | Less than or equal to 0.60 | 4.00-6.00 | 0.45-0.60 | Less than or equal to 0.60 | - | Less than or equal to 0.030 | Less than or equal to 0.020 |
| 15CrMo | 0.12-0.18 | 0.17-0.37 | 0.4-0.7 | 0.8-1.10 | 0.4-.0.55 | Less than or equal to 0.30 | - | Less than or equal to 0.035 | Less than or equal to 0.035 |
Mechanical properties of 15CrMo steel plate:
| 15CrMo | 440-640 | 235 | 21 |